Aluminum 5052
Higher fatigue strength than 3003. Excellent corrosion resistance.
Reference properties
- Category: Aluminum
- Density: 0.097 lb/in³
- Yield strength: 28,000 psi
- Tensile strength: 33,000 psi
Available tempers and conditions
- H32 — 60 HB
- Strain hardened & stabilized. Common sheet.
- O — 47 HB
- Annealed. Softest state.
The condition on the purchase order changes forming behavior as much as the alloy does. Aluminum 5052 is stocked in 2 listed conditions; confirm which one the certification covers before committing die clearance, bend radius, or press tonnage.
Production use
As an aluminum product, Aluminum 5052 should be compared against other grades in the same family before substituting — density drives coil and part weight, while the yield and tensile basis above drive forming load and springback.
Published families and nominal properties vary by grade, temper, thickness, processing history, and governing specification. Confirm the actual purchase specification and material certification before releasing a die, forming process, weld procedure, or production setup. Surface condition, grain direction, coating, work hardening, edge quality, and lot-to-lot variation can affect performance even when nominal strength values match.
Where to source Aluminum 5052
Supplier listings are starting points for availability and data sheets, not endorsements or current pricing.
Verification checklist
Verify units, thickness tolerance, yield and tensile basis, and any temperature or direction dependence. Run a representative trial when forming limits, safety, or high production volume make an incorrect assumption costly. This page is a reference, not a material certification or supplier guarantee.
Estimate cost with the material cost calculator, check coil and blank weight with the sheet weight calculator, or return to the production material library.